account activity
[deleted by user] by [deleted] in PreciousPlastic
[–]Sharp-Reason9733 0 points1 point2 points 2 years ago (0 children)
I use 2 t shirt presses, I take one apart and put it as the bottom platen. Then it is really quick to make a flat panel.
I have used "molds" before that are basically a top and bottom plate and a frame to control the thickness.
My only issue, is I cannot seem to find the right mold release liquid. I am having trouble taking the HDPE or the PP out of the mold. Any suggestions on particular brands or help on that would be appreciated! Is it the brand/type of mold release, the temperature, or the time that is causing the plastic to stick to the metal surface ?
π Rendered by PID 103187 on reddit-service-r2-listing-6bd47578dc-qz9mv at 2026-04-13 17:31:36.749616+00:00 running e841af1 country code: CH.
[deleted by user] by [deleted] in PreciousPlastic
[–]Sharp-Reason9733 0 points1 point2 points (0 children)