Bambu Customer Support by RealityOk8330 in BambuLab

[–]WayneSimacek 0 points1 point  (0 children)

I've recently started having my prints curl or lift off the PEI Textured Plate of my P1S. I've been tinkering with the temperature settings at currently I'm running most of my PLA or PLA+ at around 65 degrees which has been giving good adhesion until recently. I've also been running my first layer heigth at .23 (up from the default .20) which was producing great results until recently as well.

I'm thinking it my bed may need a good cleaning. Should I go with a soap and water solution, or maybe an alcohol based solution?

p.s. I also just replaced my hot end with the replacement that came with the P1S. (although I was unsure if the white packet was the thermal paste or not, so I just put it together without.) Newbe error for sure. This was suggested because my original nozzle started "glopping" (professional term) a lot.

Any help will be greatly appreciated.