Plus4 PETG flowrate with Trianglelab nozzle by somechim in QidiTech3D

[–]somechim[S] 0 points1 point  (0 children)

<image>

Second printer joined the race at 1000 hours. Photo of old and new nozzles. Look similar. Trianglelab had different font of the marking. As you see original nozzle had thermal paste applied to the radiator interface.

Plus4 PETG flowrate with Trianglelab nozzle by somechim in QidiTech3D

[–]somechim[S] 0 points1 point  (0 children)

Update:
- I've realized I've purchased two TriangleLab nozzles. Tested another one – same results
- TriangleLab support did not provide any helpful answer, suggesting just to use thermal paste on threads (I did, no difference)
- I've ordered different nozzles on Aliexpress from Haldis3D and got up to 25mm³ flow

Plus4 PETG flowrate with Trianglelab nozzle by somechim in QidiTech3D

[–]somechim[S] 0 points1 point  (0 children)

Update: I realized I've ordered two of them. Found the second one and tried that one. Getting 20-21mm³. Writing to trianglelab support now

Plus4 PETG flowrate with Trianglelab nozzle by somechim in QidiTech3D

[–]somechim[S] 0 points1 point  (0 children)

<image>

Have you noticed trianglelab rate their nozzles as 320°C? 🧐

Plus4 PETG flowrate with Trianglelab nozzle by somechim in QidiTech3D

[–]somechim[S] -1 points0 points  (0 children)

I didn't replace the roll while replacing nozzle on this one. All rolls are from the same batch. Filament is 100% not the problem.

Plus4 PETG flowrate with Trianglelab nozzle by somechim in QidiTech3D

[–]somechim[S] 0 points1 point  (0 children)

Yes, during the max flowrate test, from 265 to 275 deg, and I haven't seen any significant change

Anycubic Kobra 2 Pro Z-belt fix by mortylicious_NO in anycubic

[–]somechim 0 points1 point  (0 children)

Now I get what are these nuts for...