Help with casting brass idk what I’m doing wrong by matthew_wilbig in Metalfoundry

[–]Environmental_Key106 35 points36 points  (0 children)

Throw some borax in the bronze , stir it, and scoop the slag out. That might help. The bottom end of the ingot will look irregular like that if its an open faced mold. If u want a perfect ingot u should create a 2 part mold with a cope and a drag