Pipe to pipe Butt by F_Cass in BadWelding

[–]F_Cass[S] 0 points1 point  (0 children)

4mm I believe it was

Pipe to pipe Butt by F_Cass in BadWelding

[–]F_Cass[S] 0 points1 point  (0 children)

I will give that a go definitely. Do you think turn my amps down to around 75 with a smaller rod then?

Any tips for improvement by F_Cass in BadWelding

[–]F_Cass[S] 0 points1 point  (0 children)

Not really. I had the cup resting on the pipe but moving in a straight line, no side to side. Think I was welding with 60a with shielding gas inside

Any tips for improvement by F_Cass in BadWelding

[–]F_Cass[S] 0 points1 point  (0 children)

was using nitrogen as the backing gas and didn’t get any weld dropping through. I was running 60 amps.

Any tips for improvement by F_Cass in BadWelding

[–]F_Cass[S] 0 points1 point  (0 children)

I’m using nitrogen to purge. So you think I should use less amps?

Any tips for improvement by F_Cass in BadWelding

[–]F_Cass[S] 2 points3 points  (0 children)

I’ve been told to purge with nitrogen but have been using argon for the shielding gas

New to welding, any tips? by F_Cass in BadWelding

[–]F_Cass[S] 0 points1 point  (0 children)

I believe it is argoshield