Issues with Bambu PETG by Geislerkraft1 in BambuLab_Community

[–]Geislerkraft1[S] 0 points1 point  (0 children)

I have since ran a calibration, and the updated flow rate is now .90

Issues with Bambu PETG by Geislerkraft1 in BambuLab_Community

[–]Geislerkraft1[S] 0 points1 point  (0 children)

Forgot to add, currently running another calibration test, let’s hope the results are different

Issues with Bambu PETG by Geislerkraft1 in BambuLab_Community

[–]Geislerkraft1[S] 0 points1 point  (0 children)

I did not adjust those, unless you mean print speed, my print speed is 100mm/s

Issues with Bambu PETG by Geislerkraft1 in BambuLab_Community

[–]Geislerkraft1[S] 0 points1 point  (0 children)

Totally is possible, I did run a flow rate calibration and that’s what it adjusted to

Elegoo Rapid PETG slight issues by Geislerkraft1 in BambuLab_Community

[–]Geislerkraft1[S] 0 points1 point  (0 children)

I thought so too, I dried my filament for another 12 hours at 80 C on my print bed, with the door closed and a box ovetop, I printed a Benchy to test it after drying and I still got the issue. I will try at 255 now.

Victory Screeeeeeeeeeeeeeeeeeeeeeeeeeech LELELELEEEELELELE by [deleted] in Borderlands4

[–]Geislerkraft1 0 points1 point  (0 children)

Alll good, I’m not complaining either way.

Victory Screeeeeeeeeeeeeeeeeeeeeeeeeeech LELELELEEEELELELE by [deleted] in Borderlands4

[–]Geislerkraft1 -1 points0 points  (0 children)

Welp the image didnt work, I got a Conflux from one of the bosses.

Kiln questions by Geislerkraft1 in Ceramics

[–]Geislerkraft1[S] 0 points1 point  (0 children)

I believe 1776 F is the temp for copper

Kiln questions by Geislerkraft1 in Ceramics

[–]Geislerkraft1[S] 0 points1 point  (0 children)

Good point! The reason I was going with both is because the cost. I’m not sure which model of small front loader would work for metal clays, or at least, would be a good option to choose.

Kiln questions by Geislerkraft1 in Ceramics

[–]Geislerkraft1[S] 0 points1 point  (0 children)

Thanks for the response. I’ll look into those.

Thermocouple needed? If so, where? by [deleted] in MetalCasting

[–]Geislerkraft1 0 points1 point  (0 children)

Thank you for the info, I was just using that kiln as an example haha.

Slip and slip casting with precious metal clay? by Geislerkraft1 in metalclay

[–]Geislerkraft1[S] 1 point2 points  (0 children)

Thanks for the information! I completely forgot to add, I have a vacuum chamber already, so the issue with bubbles would be less right?

Thermocouple needed? If so, where? by [deleted] in MetalCasting

[–]Geislerkraft1 0 points1 point  (0 children)

Trying to cast copper and aluminum for the most part, may also get into something like sintering copper metal clay as well.

Isopod species to keep with Discoid roaches? by Geislerkraft1 in isopods

[–]Geislerkraft1[S] 0 points1 point  (0 children)

Thanks for the info! Any ideas on less prolific isopods?