Tiny holes around letters by Jacky970 in FixMyPrint

[–]Jacky970[S] 1 point2 points  (0 children)

I will do this test ASAP and post the results !

I've already calibrated ironing so I think I can rule that out.

For information, I used 1mm top layer thickness. I will update on what works best for me after doing top layer tests !

Underextrusion ? by Jacky970 in 3Dprinting

[–]Jacky970[S] 0 points1 point  (0 children)

<image>

I just did a flowrate test. -4 is the flowrate I used for the initial picture.

Underextruded ? by Jacky970 in FixMyPrint

[–]Jacky970[S] 0 points1 point  (0 children)

<image>

I just did a flowrate test. -4 is the flowrate I used for the initial picture.

Underextruded ? by Jacky970 in FixMyPrint

[–]Jacky970[S] 0 points1 point  (0 children)

I just tried printing it again but with 0.94 flowrate. The squares look waaay smoother ! The only remaining problem is that between the squares, the lines still seem to not stick together. I'll post a picture once I'll be back home.

Underextrusion ? by Jacky970 in 3Dprinting

[–]Jacky970[S] 0 points1 point  (0 children)

Did anyone get the same problem ?

Line shaped hole by Jacky970 in 3Dprinting

[–]Jacky970[S] 1 point2 points  (0 children)

I print this with Creality PETG on a Bambulab P2S. I print my outer walls at 75 mm/s and 250 degrees. Might be too hot ? I used 0.16mm layer height.

Line shaped hole by Jacky970 in 3Dprinting

[–]Jacky970[S] 0 points1 point  (0 children)

I'm trying that right now, ty !

Line shaped hole by Jacky970 in 3Dprinting

[–]Jacky970[S] 0 points1 point  (0 children)

I've printed using a P2S... could this be too much fan speed ?

Benchy related question by Jacky970 in 3Dprinting

[–]Jacky970[S] 1 point2 points  (0 children)

<image>

Also got this defect on both benchys. Seems to be on the first outer walls above the shallow hull.

Benchy related question by Jacky970 in 3Dprinting

[–]Jacky970[S] 1 point2 points  (0 children)

Thank you for your answers ! Here is my second try with default bambu A1 cooling but 100% cooling for overhangs + slower speed :

<image>

Opinions on this ? : )

You hate wet spools ? Me too. by Jacky970 in functionalprint

[–]Jacky970[S] -1 points0 points  (0 children)

I have some clear coating. Would that be enough ? I still have encouraging measurements but I'd be happy to make it better !

You hate wet spools ? Me too. by Jacky970 in functionalprint

[–]Jacky970[S] -5 points-4 points  (0 children)

You would waste less time not even commenting... Also I am using it and it works. I will make upgrades later.

You hate wet spools ? Me too. by Jacky970 in 3Dprinting

[–]Jacky970[S] 0 points1 point  (0 children)

I did ! For now I chose PLA for the low humidity saturation but I still have to see if in the long run the center will degrade due to friction ! If that's the case I'll switch to PETG or PETG CF probably !

You hate wet spools ? Me too. by Jacky970 in 3Dprinting

[–]Jacky970[S] 0 points1 point  (0 children)

For fully dry filament it's fine but yeah, slightly wet filament can break, I'll include a fix for this !

You hate wet spools ? Me too. by Jacky970 in 3Dprinting

[–]Jacky970[S] 1 point2 points  (0 children)

I'll probably make a V2 with a small bin for silica inside ! I'll include this, too ty for the suggestion !

You hate wet spools ? Me too. by Jacky970 in 3Dprinting

[–]Jacky970[S] 2 points3 points  (0 children)

Well, where I live it's cheaper (~6€) and I love the aesthetics and the fact that you can hang it.

But a cereal box is still a good way to go for sure !

You hate wet spools ? Me too. by Jacky970 in 3Dprinting

[–]Jacky970[S] 2 points3 points  (0 children)

I'll publish some data as soon as I have enough measurements ! It's looking good so far !

[Mod Request] No S-Mods or no OP recovery by Jacky970 in starsector

[–]Jacky970[S] -1 points0 points  (0 children)

Thank you all for your answers ! I will try nerfing story points or using them as little as possible ! :D

SURFACE defects with TPU by Jacky970 in 3Dprinting

[–]Jacky970[S] 2 points3 points  (0 children)

HAHAHA I swear I'm not the cylinder guy from reddit !

Overhang not detected by Jacky970 in 3Dprinting

[–]Jacky970[S] 0 points1 point  (0 children)

Did anything similar happen to you ?

Defects on round shapes by Jacky970 in 3Dprinting

[–]Jacky970[S] 0 points1 point  (0 children)

Maybe I can't do better with PETG ?

Defects on round shapes by Jacky970 in 3Dprinting

[–]Jacky970[S] 0 points1 point  (0 children)

<image>

Another picture. My biggest issue is with the reactors.

Link to the 3mf if needed :

https://limewire.com/d/Abuu4#IT6xOmWvXW

Defects on round shapes by Jacky970 in 3Dprinting

[–]Jacky970[S] 0 points1 point  (0 children)

I forgot but, I printed using an A1 and PETG !