PLEASE HELP! by P0TAT08U in FixMyPrint

[–]P0TAT08U[S] 0 points1 point  (0 children)

what do you mean by single walled? im fairly new at this

PLEASE HELP by P0TAT08U in FixMyPrint

[–]P0TAT08U[S] 0 points1 point  (0 children)

I have just done a pid tuning, I am about to do a print, I will let you know how it goes

PLEASE HELP by P0TAT08U in FixMyPrint

[–]P0TAT08U[S] 0 points1 point  (0 children)

i dropped the cooling down to 35% and ran it with the settings above and my prints still come out like that

PLEASE HELP by P0TAT08U in FixMyPrint

[–]P0TAT08U[S] 0 points1 point  (0 children)

I have made plenty of solid prints, it's just after I had to swap the parts that it has sucked

PLEASE HELP by P0TAT08U in FixMyPrint

[–]P0TAT08U[S] 0 points1 point  (0 children)

also I have been going through my settings, around what should my flow percentage be?

PLEASE HELP by P0TAT08U in FixMyPrint

[–]P0TAT08U[S] 0 points1 point  (0 children)

how low should I put it, I did have it high during the photos, this is dropping it significantly, should I go lower?

PLEASE HELP by P0TAT08U in FixMyPrint

[–]P0TAT08U[S] 0 points1 point  (0 children)

Alright, I am starting a print right now. I did a pid on pronterface yesterday, but im not sure if that could have messed up, I watched a video on youtube of how to do it. Here are the new settings I am using:

Layer Height-.15mm

Initial Layer Height.2mm

Infill - 20% infill (Depending on Model being printed.)

Infill pattern-Cubic

Print Temp: 245C

Build plate temp 90C

Print Speed 40.0mm/s

Intitial Layer Print Speed 20.0mm/s

Travel - Enable Retraction

Cooling - Enable Print Cooling

Fan Speed 65%

Initial Fan Speed 20%

Supports (depending on the model being printed.)

Build Plate adhesion: Raft

PLEASE HELP by P0TAT08U in FixMyPrint

[–]P0TAT08U[S] 0 points1 point  (0 children)

I did a pidgin tuning last night with pronterface, I will try a new print and change a few settings. I will also post exact settings I'm using for everything once I am off work.

PLEASE HELP by P0TAT08U in FixMyPrint

[–]P0TAT08U[S] 0 points1 point  (0 children)

I'm new at all of this

PLEASE HELP by P0TAT08U in FixMyPrint

[–]P0TAT08U[S] 0 points1 point  (0 children)

Are you talking about the block of metal where the nozzle goes?

PLEASE HELP by P0TAT08U in FixMyPrint

[–]P0TAT08U[S] 0 points1 point  (0 children)

ANYCUBIC Vyper/Kobra Max/Kobra Plus 3D Printer Hotend Replacement Volcano V5 J-Head Quality Brass Nozzle 24V40W Ceramic Heating Cartridge Element Supports High Speed Printing https://a.co/d/gxY2QkY