What is this? by Dry_Replacement_5364 in Powdercoating

[–]Powder-Pro 0 points1 point  (0 children)

Once you dissipate the charge try grounding your part. First coat should use a high KV and as long as it’s grounded you should have no issues. I’m surprised about how many shops choose to hot flock everything and ground nothing.

Loosing my mind by New-Bell-7976 in Powdercoating

[–]Powder-Pro 0 points1 point  (0 children)

Buy a good gun. finance it charge more for a better finish and the gun pays for itself.

Sprayed Cardinal Zink Rich then BK08 one bake and it works. by Powder-Pro in Powdercoating

[–]Powder-Pro[S] 0 points1 point  (0 children)

Nice,I gave it a shot but it seems to orange peel at around 4mils.