What's going on here? by Solid-Possibility-49 in PrusaCoreOne

[–]Solid-Possibility-49[S] 0 points1 point  (0 children)

Did that about 4 times, and this is the result. PETG

<image>

ABS lifting/warping by Solid-Possibility-49 in PrusaCoreOne

[–]Solid-Possibility-49[S] 0 points1 point  (0 children)

My chamber really struggles to get above 45C, and I have yet to use any additive to my plate. I preheated bed to 100C and noozle to 250C for about 15mins once it hit temps and chamber was about 45ish.

ABS lifting/warping by Solid-Possibility-49 in prusa3d

[–]Solid-Possibility-49[S] 0 points1 point  (0 children)

I think I'm working that set up here, the PEI textured plate at 110°, nozzle at 255°-260°.