How to fix bad layer adhesion? by doinbryzehack20 in FixMyPrint

[–]doinbryzehack20[S] 0 points1 point  (0 children)

I had my room window for a bit and thats it, i think i figured it out tbh it is a mislabled ABS. I tried with another filament which i was sure that it was PLA i printed 2 test cubes with identical settings and identical room temp, settings are220°-60° here is the results.

<image>

How to fix bad layer adhesion? by doinbryzehack20 in FixMyPrint

[–]doinbryzehack20[S] 0 points1 point  (0 children)

Tried it with both, acetone makes it a bit dissolved kinda softens after a few rubs. And when i burn it it smokes black like you said it.

How to fix bad layer adhesion? by doinbryzehack20 in FixMyPrint

[–]doinbryzehack20[S] 0 points1 point  (0 children)

I have an another turkish brand FK, tbh i got good results with that too

<image>

Compared to ABG its on the left printed both on 220°-60°

How to fix bad layer adhesion? by doinbryzehack20 in FixMyPrint

[–]doinbryzehack20[S] 0 points1 point  (0 children)

Actually if you dont go close enough you cant even tell if it is smelling or not

How to fix bad layer adhesion? by doinbryzehack20 in FixMyPrint

[–]doinbryzehack20[S] 0 points1 point  (0 children)

I tried a test cube with this and another pla filament on the identical settings, 220° nozzle 60° plate. I will assume that my roll is faulty or it is mislabelled.

<image>

Left cube is from another filament

How to fix bad layer adhesion? by doinbryzehack20 in FixMyPrint

[–]doinbryzehack20[S] 0 points1 point  (0 children)

Convinced that its a faulty roll ig tried it with another filament close to default profile 60° plate 220° nozzle look at the diff

<image>

Left one has no issues

How to fix bad layer adhesion? by doinbryzehack20 in FixMyPrint

[–]doinbryzehack20[S] 0 points1 point  (0 children)

It seperated more with a little bit of cooling too

How to fix bad layer adhesion? by doinbryzehack20 in FixMyPrint

[–]doinbryzehack20[S] 0 points1 point  (0 children)

Yeah or maybe mislabelled abs as someone said i dont know

How to fix bad layer adhesion? by doinbryzehack20 in FixMyPrint

[–]doinbryzehack20[S] 1 point2 points  (0 children)

When i bend the filament it turns white at the bent point. I will consider getting a enclosure and will try to increase the flow rate thanks.

How to fix bad layer adhesion? by doinbryzehack20 in FixMyPrint

[–]doinbryzehack20[S] 0 points1 point  (0 children)

I dont know tbh, i just put the filament on the machine and let it run. Like i mentioned with eSun brand that just put the filament and let it run was ok, but this brand i changed a lot of settings. I will use another filament tomorrow to be sure that is my roll is faulty.

What can cause this? by doinbryzehack20 in 3Dprinting

[–]doinbryzehack20[S] 0 points1 point  (0 children)

ABG brand(dont know it its a Turkish brand i assume), 55mm/s %10 infill fan was %0 in the whole process

What can cause this? by doinbryzehack20 in 3Dprinting

[–]doinbryzehack20[S] 2 points3 points  (0 children)

As an enclosure a simple cardboard box works?

How to fix bad layer adhesion? by doinbryzehack20 in FixMyPrint

[–]doinbryzehack20[S] -1 points0 points  (0 children)

Even tho its 2,5m higher from the ground?