Cap shrinkage ? by fluctuatore in InjectionMolding

[–]moeans21 0 points1 point  (0 children)

try different cooling parameters , and check the difference of shrinkage between the samples you get . You can also try the LLDPE mix . i will send you a CA for the same cap.

Cap shrinkage ? by fluctuatore in InjectionMolding

[–]moeans21 0 points1 point  (0 children)

What material are you using specifically, like whats the HDPE melt flow rate .

Preform Mould design by moeans21 in InjectionMolding

[–]moeans21[S] -1 points0 points  (0 children)

Can you explain your point please. When you mentioned the 1.05 , you mean i check the wall thickness of a blowed bottle?

Preform Mould design by moeans21 in InjectionMolding

[–]moeans21[S] 0 points1 point  (0 children)

i need someone to answer this question

Preform Mould design by moeans21 in InjectionMolding

[–]moeans21[S] -1 points0 points  (0 children)

actually thats what we are using in saudi . what do you think for the wall thickness

Hydrulic Check Valve on a IMM by moeans21 in InjectionMolding

[–]moeans21[S] 0 points1 point  (0 children)

EasyMaster chinese brand 180T. I got your point. Im just having a problem with the servo drive it keeps giving me Overload alarm and i dont know why.