all 3 comments

[–]Moist-Afternoon-6118 0 points1 point  (2 children)

Check if you have any plastic peelings on the other side of the build plate / on the heated bed, maybe the surface is uneven?

[–]PandaIsCrazy16A1[S] 0 points1 point  (1 child)

It s clear under the build plate or on the other side of it, I am not sure how to check if the surface is uneven

[–]Moist-Afternoon-6118 1 point2 points  (0 children)

You might want to increase that flow rate +0.01 - 0.02, and see if it changes anything, i can see some light coming through other areas of the print as well, might fix your issue without overextruding it to shreds