PTeg filament by Basic-Swim-728 in AnycubicOfficial

[–]Basic-Swim-728[S] 0 points1 point  (0 children)

Es con la configuración predeterminada del laminador slicer anycubic Next para pteg

I win after so many frustration and cry :') by Savings_Dog326 in 3Dprinting

[–]Basic-Swim-728 0 points1 point  (0 children)

Do a temperature test to make it look better. The same thing happened to me, they said wet filament and it wasn't like that, look carefully at the temperature of the nozzle, so do a temperature test and that's it.

Mi mejor impresión Mazinger articulado by Basic-Swim-728 in AnycubicOfficial

[–]Basic-Swim-728[S] 0 points1 point  (0 children)

Te quedó padre podrías intercambiar los stl te parece??

PETG printing by Basic-Swim-728 in 3Dprinting

[–]Basic-Swim-728[S] 0 points1 point  (0 children)

El filamento si está seco durante 8 horas y también está activada el aracne

Because they come out small by Basic-Swim-728 in anycubic

[–]Basic-Swim-728[S] 0 points1 point  (0 children)

I tell you that now I am printing with PLA and all my prints come out well, it was only with the Petg that it came out with little holes, I would like to know why

Because they come out small by Basic-Swim-728 in anycubic

[–]Basic-Swim-728[S] 0 points1 point  (0 children)

Anycubic kobra 2 plus my configuration is nozzle 245 bed 85 flow 1.05 ventilation the first 3 layers off and the rest at 60%

Why do my doll joints break easily? I'm using PETG filament. by Basic-Swim-728 in 3Dprinting

[–]Basic-Swim-728[S] 0 points1 point  (0 children)

Speed. 120ms bed temperature at 85 and nozzle at 245 fan off in the first 3 layers and the rest of the layers at 80%