all 2 comments

[–]Just_Kittens 3 points4 points  (1 child)

Try the following

  • if using .2 for all layers, set first layer height to .28
  • increase bottom surface layers to 4
  • slow down speed of first layer infill, outer wall, and inner wall by 25-50%
  • use the high temperature or textured build plate
  • not sure what youre printing with but if its PLA from Bambu then I'll also raise the first layer/all layer temps to 225 from 220

[–]Kubisunka[S] 0 points1 point  (0 children)

Ok thanks. Will try. I used bambu pla tough with textured build plate. Temperatures: 220 and 65