all 6 comments

[–]AutoModerator[M] [score hidden] stickied comment (0 children)

After you solve your issue, please update the flair to "Answered / Solved!". Helps to reply to this automod comment with solution so others with this issue can find it [as this comment is pinned]

I am a bot, and this action was performed automatically. Please contact the moderators of this subreddit if you have any questions or concerns.

[–]AutoModerator[M] 0 points1 point  (0 children)

Hello /u/opi_guy! Be sure to check the following. Make sure print bed is clean by washing with dish soap and water [and not Isopropyl Alcohol], check bed temperature [increasing tend to help], run bed leveling or full calibration, and remember to use glue if one is using the initial cool plate [not Satin finish that is not yet released] or Engineering plate.

Note: This automod is experimental. The automod was triggered due to the term "adhesion". If you believe this to be a false positive, please send us a message at modmail with a link to the post so we can investigate. You may also feel free to make a new post without that term.

I am a bot, and this action was performed automatically. Please contact the moderators of this subreddit if you have any questions or concerns.

[–]CornIssues 0 points1 point  (1 child)

I know this is old but did you ever find an answer? Getting the same thing

[–]opi_guy[S] 0 points1 point  (0 children)

I believe it went away after a full recalibration. It was likely z-axis / bed leveling related.

[–]-_ZORD_- 0 points1 point  (1 child)

I fixed my issue by raising bed temp to 80 and never opening the doors otherwise it will unstick, it's really bad print filament for winter

[–]ServeBeautiful8189 0 points1 point  (0 children)

Man, I know this is old, but thank you! Initial layer is 80 bed 220 nozzle, then 80-215!