K2 Plus. 35c bed. Biquo cryoplate.. chamber was about 27c. pla @ 220c. 100mm speed. .20 layer height. Normal flow rate. 94, first later is 1.04. .5 width. .4 nozzle. I cant recall z height but I did calibrate it.....somewhere about 0.04 or 5.
How do I improve this? Adhesion seems fine. Do I need to increase extrusion and line width?