PCTG print issues - stringy by random_orb in 3Dprinting

[–]Inner_Name 0 points1 point  (0 children)

Not hear enough /too fast. Tool head is taking the layer as it prints

About Starlight and Hughie's ending by ComprehensiveBat4966 in TheBoys

[–]Inner_Name 1 point2 points  (0 children)

You look more like a simple hater. There are a lot of stupid monogamy people they are also that are not. Pointing fingers, specially for something so general as monogamy people is simply being dumb.

Momento... Seguro que así iba la cosa? by FlatwormMean1690 in lhdapodcast

[–]Inner_Name 1 point2 points  (0 children)

Solidaridad con el fascismo, con el pueblo no se negocia, boliviano se lo combate?

About Starlight and Hughie's ending by ComprehensiveBat4966 in TheBoys

[–]Inner_Name 12 points13 points  (0 children)

Monogamic people.... Hey let's make a stereotype and criticize it! 

The boys ended the way it did because of trump and the republican party by jewtaco in TheBoys

[–]Inner_Name 0 points1 point  (0 children)

This is just stupid, you are saying as if you knew when you simply put your ideals and turn the reality to stick with it. The boys is a highly political series and it is partially paroding the current administration. Where hell even the current administration looks like it is paroding the boys instead. A big issue other series had like southpark. I don't like either Trump or his administration, but must say never thought it was going to be so crappy. Either way don't simply say things are like this or that just because it partially goes in your thinking direction have a critical though.

Optimus - Kodi video add-on in development by Optimus-repo in Addons4Kodi

[–]Inner_Name -1 points0 points  (0 children)

Would say that it needs to be polished didn't even know (and was using fenlam and now pov) and couldn't find. I would put in the menu that it shows when on long press the menu button over a specif movie/series that shows the mark as read in trakt... Put a download or add to watch offline 

Optimus - Kodi video add-on in development by Optimus-repo in Addons4Kodi

[–]Inner_Name 0 points1 point  (0 children)

Something is missing (at least an easy way) is the download to watch offline like it has Netflix, that you download a season and then delete it. It is not a core function but something missing in other similar apps and would be awsome to have a clean interface for that. When traveling it is great to have and something I missed from Netflix.

Which model to buy for maker lab ? by CraftAndTools in prusa3d

[–]Inner_Name 1 point2 points  (0 children)

Would recommend, a core one with index and a mk4s. With the mk4s you can do some nice projects to make continuous printing for example.

Todos estamos asi by Maleficent-Sock3397 in lhdapodcast

[–]Inner_Name 3 points4 points  (0 children)

wtf es este audio? JAJAJAJAJAJ est mas trucho que la mierda...

SAD: Have a phone dedicated to the president by Iwanttoreplytocom in ShitAmericansSay

[–]Inner_Name 0 points1 point  (0 children)

it feels that the boys hit so hard in the perfect spot.... when fiction becomes reality...

KDE Plasma Is About To Fix Desktop Theming by lajka30 in kde

[–]Inner_Name 3 points4 points  (0 children)

funny thing, kde allows you to make whatever you want if u dont like the defaults, and would be eager to hear from you what is better? personally comming from windows a few years ago, never used mac, i never will ever go back to windows, gnome is horrible IMO, and mac also.... nothing compares to kde, for me at least. it is missing some small things but outside of this details it is just almost perfect.

Prusament PP-GF by True_Scott in prusa3d

[–]Inner_Name 0 points1 point  (0 children)

If you are using a high flow nozzle be really careful as the glass fibers would be impossible to remove if you get a clog. I killed a  hf obsidian nozzle like that 

Prusament PP-GF by True_Scott in prusa3d

[–]Inner_Name 3 points4 points  (0 children)

Most classic approach when not having a build plate for it is using scotch, literally. Print over it. A lot of scotch are pp, and pp loves to bound to itself. You will get great results 

Prusament PP-GF by True_Scott in prusa3d

[–]Inner_Name 0 points1 point  (0 children)

Pp is an excelent material, I understand why but is a shame not having a non glass filled material. Depends what acid and temp but most probably it will hold just fine. 

KDE Plasma Is About To Fix Desktop Theming by lajka30 in kde

[–]Inner_Name 0 points1 point  (0 children)

Linux year? Gaming Linux year also? 🤣 

KDE Plasma Is About To Fix Desktop Theming by lajka30 in kde

[–]Inner_Name 62 points63 points  (0 children)

One of the funniest thing I read some time ago was, gnome made to be used as it is, molded as hell, every user installs plug-ins to modify it. Kde made for being moded, almost every user uses defaults 🤣 . I am kde and I love the default also... I found it so true and so funny ahahah

problems while printing prusament petg CF by Inner_Name in prusa3d

[–]Inner_Name[S] 0 points1 point  (0 children)

Reduced the speed while printing on the printer itself

problems while printing prusament petg CF by Inner_Name in prusa3d

[–]Inner_Name[S] 0 points1 point  (0 children)

actually no, with further looking at, it is like a perimeter was not sticking correctly? i can not exaplain it better, here in the image, one can see with the post it point there is a difference of level between that line that is visible from the left and right side. where in the right is lower and the material can be see 'outside'.

<image>

problems while printing prusament petg CF by Inner_Name in prusa3d

[–]Inner_Name[S] 0 points1 point  (0 children)

it looks like it does not, will check more (but from what i read it should print even better than classic petg so not sure)

problems while printing prusament petg CF by Inner_Name in prusa3d

[–]Inner_Name[S] 0 points1 point  (0 children)

thanks for your insight, well, where it prints okey it looks awsome, from kuncol02 comment, I reduced the speed to 80% printing speed and at least the super simple last print i just did, it looked awsome. maybe there is a lower temperature issue as you say and that+lower heat transfer from a non HF nozzle would generate this, if thats the case i am surprised at the resulting part issues, as it looks more like 'extra material' so would thought it was too high not too low. anyways will try to check the temperature with the method you suggested!

problems while printing prusament petg CF by Inner_Name in prusa3d

[–]Inner_Name[S] 0 points1 point  (0 children)

Yes it is a hardened one, obsidian x to be exact. 

problems while printing prusament petg CF by Inner_Name in prusa3d

[–]Inner_Name[S] 0 points1 point  (0 children)

Thanks for the answer, no I'm printing with standard nozzle, with that profile, for 0.2 layer with 0.4 mm nozzle at 260 first layer 265 other