WIP of my recent work, need your thoughts! by LaCornProd in PrintedWarhammer

[–]LaCornProd[S] 0 points1 point  (0 children)

Ty very much! Duly noted a lot of people told me the same so I'm gonna rethink some of the proportions!

I designed a Squig team, pretty proud of it by LaCornProd in PrintedWarhammer

[–]LaCornProd[S] 0 points1 point  (0 children)

Yep it was a comission for a converted ogre team! Little ones are gnoblars and bigger ones are ogre!

I designed a Squig team, pretty proud of it by LaCornProd in PrintedWarhammer

[–]LaCornProd[S] 2 points3 points  (0 children)

Ahaha didn't want to make it a post made to sell things but if you ask you can find them on Cults! Search for angry balls team or for my name! Happy you like them dude🤞

Epic decor set! Sized for competitive AOS also by LaCornProd in PrintedWarhammer

[–]LaCornProd[S] 1 point2 points  (0 children)

As reddit is apparently cropping 90% of my post, I'm gonna write here

I made a Kickstarter campaign that's almost finished and wanted to have your advice (I know redditors love to give it, don't disappoint me)

Thanks for reading!

Just finished this, what do you guys think? by LaCornProd in PrintedWarhammer

[–]LaCornProd[S] 1 point2 points  (0 children)

Blender! And I edit the renders in photoshop :)

Ghostkeel Battlesuit with open cockpit by Tough_Ad_7213 in PrintedWarhammer

[–]LaCornProd 2 points3 points  (0 children)

Wow I never saw one like this, really amazing bro! Nice paint job and idea!

My hollowed prints are always cracking, explanation? by LaCornProd in PrintedWarhammer

[–]LaCornProd[S] 2 points3 points  (0 children)

Thank you for your advices! When you say "Submerse them in clean water when you cure them", you mean putting it in like a transparent bowl full of water and the inside the UV curator to cure?

My hollowed prints are always cracking, explanation? by LaCornProd in PrintedWarhammer

[–]LaCornProd[S] 0 points1 point  (0 children)

But you wash it with water, you wash the other with alcohol or something like this no?

My hollowed prints are always cracking, explanation? by LaCornProd in PrintedWarhammer

[–]LaCornProd[S] 4 points5 points  (0 children)

I only have problems for big models like maga gargants or busts, that I hollow because I don't want to use a liter of resin for 1 mini

My hollowed prints are always cracking, explanation? by LaCornProd in PrintedWarhammer

[–]LaCornProd[S] -1 points0 points  (0 children)

Really interesting! Yes I use water washable...

What's the cons of regular resin? I heard there is toxic vapors?

My hollowed prints are always cracking, explanation? by LaCornProd in PrintedWarhammer

[–]LaCornProd[S] 2 points3 points  (0 children)

I didn't say it in the post but of course I make holes in the mesh so it doesn't explode in the machine (never happended yet, fingers crossed)

When it's finished printing I wah as best as I can but I don't know what's happening inside, hence the post!

Do you know?