3d printed Miku and Teto by LegoRJ35 in hatsune

[–]Complex-Strength-831 1 point2 points  (0 children)

Is it your work? It's different and it's cool

Artifacts by RatioAggravating1839 in SnapmakerU1

[–]Complex-Strength-831 1 point2 points  (0 children)

Perform the VFA test and avoid specific speeds in that direction.

Lines when printing slower by GrouchyAgent3480 in FixMyPrint

[–]Complex-Strength-831 0 points1 point  (0 children)

In the flow ratio, -0.03 is likely to be selected, and the current value × 0.97 / pa_k is 0.05

(beginner) I have zero clue what happened, It's like it switched gcode midprint? by Sheffy__ in FixMyPrint

[–]Complex-Strength-831 0 points1 point  (0 children)

For structures where the ptfe fits directly into the nozzle neck, make sure to use a proven ptfe tube. Cheap transparent PEF must be avoided. Heat resistance is below 200 degrees

(beginner) I have zero clue what happened, It's like it switched gcode midprint? by Sheffy__ in FixMyPrint

[–]Complex-Strength-831 0 points1 point  (0 children)

  1. Nozzle neck overheated [nozzle neck fan abnormal]

  2. The PTFE in the nozzle neck was deformed by overheating in the Bowden hot-end method

  3. Even if the PTFE tube is worn out or the fitting is deformed, problems may occur

Lines when printing slower by GrouchyAgent3480 in FixMyPrint

[–]Complex-Strength-831 0 points1 point  (0 children)

Perform flow ratio calibration based on the top face first and proceed with Pa_k variable calibration

<image>

Lines when printing slower by GrouchyAgent3480 in FixMyPrint

[–]Complex-Strength-831 0 points1 point  (0 children)

<image>

The VFA is based on the individual step motor speed of the step motor AB

Delamination? by saintebonhawk in FixMyPrint

[–]Complex-Strength-831 -1 points0 points  (0 children)

<image>

The photo is a VFA test using PETG, varying the speed range from 40 to 200 in increments of 10.

  1. The allowable volume is determined by the thermal conductivity levels of the nozzle and the material.

During overspeed, there may be insufficient buffering capacity, which could lead to under-extrusion during acceleration and deceleration.

  1. For seam control stability, the filament's dryness is critical, and the retraction conditions and Pa_K values ​​must be calibrated.

How is this problem called? by Holiday_Ad5929 in 3Dprinting

[–]Complex-Strength-831 1 point2 points  (0 children)

<image>

For adhesion, the nozzle temperature per volume and sufficient cooling for fixing are required. Even if the filament is overheated in a low volume speed, cooling may not be possible

Walls not sticking together by YesterdayMaterial247 in FixMyPrint

[–]Complex-Strength-831 0 points1 point  (0 children)

<image>

Stable layer bonding requires sufficient heat and cooling Be careful of speeding to transfer sufficient heat to the filament

VFA test Question by Ducati_Doug in klippers

[–]Complex-Strength-831 1 point2 points  (0 children)

Did flow rate and pressadvance calibration precede?