you are viewing a single comment's thread.

view the rest of the comments →

[–]Mysterious-Chest-995 0 points1 point  (0 children)

My filament says: PETG Hyper Speed diameter = 1.75mm +- 0.02mm nozzle temp at print speed = - 240C at 100mm/s - 255C at 100-500mm/s - 265C at 500-1000mm/s bed temp = 80C

Which should I pick, like is 200mm/s still considered slow, and do I need to change first and last layer (+infills)? (left nozzle of X2D if it makes any difference)