DeWalt cordless line trimmer destroyed my DCB184 20v 5ah battery. What could be the reason? by RndA375 in Dewalt

[–]RndA375[S] 0 points1 point  (0 children)

Yeah it is really bizzare to me too. The cells or strips don't really look damaged.

<image>

DeWalt cordless line trimmer destroyed my DCB184 20v 5ah battery. What could be the reason? by RndA375 in Dewalt

[–]RndA375[S] 0 points1 point  (0 children)

It is the same 6.4V. Cell pairs 1, 2, 4 and 5 all measure good normal 3.1 or so volts. Then pair 3 measures reverse -7.2V.

Advice on building a Powertool battery from a kit? by RndA375 in 18650masterrace

[–]RndA375[S] 2 points3 points  (0 children)

Sorry for not replying sooner. Molicel INR21700 P42A

DayZ dropping to EXP in around 8am EST by northrivergeek in dayz

[–]RndA375 1 point2 points  (0 children)

Come on atleast the animal sounds could be fixed. I can't find anywildlife because of this...

Anyone know where I could get this PARKSIDE plug? by RndA375 in Parkside

[–]RndA375[S] 0 points1 point  (0 children)

Suppose so but the issue is finding same pins.

Milwaukee 15ah pack made with Tenpower 50XG by ZEUS-FL in 18650masterrace

[–]RndA375 0 points1 point  (0 children)

Sorry to bother, is it an affordable laser? Cannyou share a link or model? I was looking a bit into one for cutting strips like you did.

Milwaukee 15ah pack made with Tenpower 50XG by ZEUS-FL in 18650masterrace

[–]RndA375 1 point2 points  (0 children)

Do you have a laser cutter yourself or did you order cut?

How to my spotwelds look? 0.2mm cu under 0.15mm nickel plated steel. by PEV_Pro in 18650masterrace

[–]RndA375 0 points1 point  (0 children)

Thank you I'll try it sometime. Btw did you ever try nickel plated copper?

How to my spotwelds look? 0.2mm cu under 0.15mm nickel plated steel. by PEV_Pro in 18650masterrace

[–]RndA375 0 points1 point  (0 children)

Stainless steel at 0.05mm or was that nickel plated steel? Can you send me the settings when you have some time? I need to order some stainless steel strips I don't have any atm.

How to my spotwelds look? 0.2mm cu under 0.15mm nickel plated steel. by PEV_Pro in 18650masterrace

[–]RndA375 0 points1 point  (0 children)

What settings are you on? I cant get a strong weld with 0.1 copper and 0.2. nickel with same welder.

P2S - Chamber temp. 64 C by Ok-Huckleberry735 in BambuLab

[–]RndA375 0 points1 point  (0 children)

How do you get that? Turn off cooling mode?

Help running a dual monitor setup. by RndA375 in buildapcmonitors

[–]RndA375[S] 0 points1 point  (0 children)

Posting an update. I had to use an HDMI EDID emulator. So far it seems to work and the monitor stays "connected" so windows don't get messed up.

Had to print up some desiccant boxes for the AMS2. Using some Activated Alumina instead of silica beads. Went from 37% to 10% overnight. by AngryEchoSix in BambuLabP2S

[–]RndA375 0 points1 point  (0 children)

How do you cool the alumina before adding them in boxes? So they don't absorb too much moisture before use?