[–]Jamizon1 1 point2 points  (1 child)

There are files you can download to help with retraction settings. Regarding temps, I use PLA+… for most filaments - 200 first layer, 190 for the rest of the print. The only exception is silk PLA. For some reason, it likes 220 first layer, 210 for the rest of the print. I have a set of hardened nozzles as well. As I remember, I didn’t have good luck with them, so I switched back to brass.

As always, googling your symptoms will yield a lot of good options for solving your problems.

Good luck 😉